ASTM A240 Grade 302 Wire Chemical Composition
Grade |
The Element Max (%)
|
||||||
C
|
Mn
|
P
|
S
|
Si
|
Cr
|
Ni
|
|
ASTM A240 302
|
0.15
|
2.00
|
0.045
|
0.030
|
0.75
|
17.0-19.0
|
8.0-10
|
Mo
|
N
|
Cu
|
|
|
|
|
|
|
0.10
|
|
|
|
|
|
Grade |
ASTM A240 302 Mechanical Property |
||||
Yield
|
Tensile
|
Elongation
|
Hardness, max
|
||
ASTM A240 302
|
Min Mpa
|
Mpa
|
Min %
|
Brinell
|
Rockwell B
|
205
|
515
|
40%
|
201
|
92
|
Japan |
USA |
Korea |
Australia |
UK |
Germany |
EU |
France |
JIS |
UNS |
KS |
AS |
BS |
DIN 17440 |
EN |
NFA35-572 |
- |
S30200 |
- |
- |
302S25 |
X12CrNi188 |
- |
Z10CN18.09 |
Uniform heating to 2100 F(1149 C) will allow Grade 302 stainless steel to be forged, upset and headed successfully. Do not work 302 below 1700 F (927 C).
Grade 302 Stainless Steel Wire Cold Working
Cold working will dramatically increase the hardness of this material, however it is quite ductile and may readily be drawn, spun and upset. Any cold work will cause this alloy to become magnetic.
Grade 302 Stainless Steel Wire Annealing
1850-2050 F (1010-1121 C) with cooling at a rapid rate to avoid the precipitation of chromium carbides.
Grade 302 Stainless Steel Wire Hardening
This alloy does not respond to heat treatment.
Shanghai Katalor Enterprises Co., Ltd is a big complex combined steel stockist whose business related with trade, processing, storage and transportation. we are specialized in supplying ASTM A240 Grade 302 Stainless Steel Wire. We have the good quality and advanced equipment, our products meet the state standard, and also available for customers' requirement. If you have any need of Grade 302 Stainless Steel Wire, please do not hesitate to contact us by email info@katalor.com, we can do our best to help you!