GB/T3094 10# Rectangular Hollow Section/Square Hollow Section Performance



C :0.07~0.13
Si:0.17~0.37
Mn:0.35~0.65
S :≤0.035
P :≤0.035
Cr:≤0.15
Ni:≤0.25
Cu:≤0.25

GB/T3094 10# Mechanical Property

Tensile strengthσb (MPa): ≥335
Yield strengthσs (MPa): ≥205
Elongation rateδ5 (%): ≥31
Section shrinkageψ(%): ≥55,
Hardness: no heat treatment,≤137HBs,
Sample size: sample size 25mm longitudinal


2017年3月29日星期三

JIS G4051-2005 S20C Steel Pipe Delivery Condition



C 0.18-0.23
Si 0.15-0.35
Mn 0.30-0.60
P≤0.030
S≤0.035


S20C Steel Pipe is used to manufacture a variety of mechanical parts that do not bear to great stress and the same time require high toughness. S20C is used in the manufacture of surface hardness requirements and the heart of the little bit of carburizing in general machinery and automobiles, agricultural machinery.

2017年3月28日星期二

42CrMo Alloy Steel Plate Current Stock Price


42CrMo Alloy can also instead of nickel-containing high-quality quenched and tempered steel

42CrMo Alloy Steel Plate Chemical Compositions

C :0.38~0.45%
Si:0.17~0.37%
Mn:0.50~0.80%
S :Allow residual content≤0.035%
P :Allow residual content≤0.035%
Cr:0.90~1.20%
Ni:Allow residual content≤0.030%
Cu:Allow residual content≤0.030%
Mo:0.15~0.25%

The Main Features of 42CrMo Alloy Steel


The performance of 42CrMo Alloy Steel is close to 35CrMo. 42CrMo Alloy Steel Plate's strength and hardenability are better than 35CrMo due to the increase in carbon and chromium content. 42CrMo Alloy Steel Plate has a high fatigue strength and resistance to multiple impact capacity after quenched and tempered. Besides, its low temperature impact toughness is good, and it is no obvious tempering brittleness.

learn more:http://www.ice-steels.com/News/42CrMo-Alloy-Steel-Plate-Current-Stock-Price.html
TEL: 0086-21-61182423
Fax: 0086-21-61182425
E-mail:service3@katalor.com 

Skype: lisa.liu6282

2017年3月24日星期五

11.30MM Thickness S355MC Steel Plate Wholesale Price


S355MC Steel Plate is widely used in bridges, vehicles, ships, construction, pressure vessels and so on.

Chemical Compositions of S355MC

Marking
Content of Elements - Mass [max%]
C max
Si max
Mn max
P max
S max
Al-celk. max
Nb max
Ti max
S 355 MC
0.12
0.50
1.50
0.025
0.020
0.015
0.09
0.15



Marking
Min. yield strength
ReH 1] [MPa]
Tensile strength
Rm[MPa]
Ductility [%]
Min A80
<3mm
Min A6
≥3mm
S 355 MC
355
430-550
19
23


TEL: 0086-21-61182423
Fax: 0086-21-61182425
E-mail:service3@katalor.com  
Skype: lisa.liu6282

2017年3月21日星期二

304 stainless steel pipe Manufacturing Process



304 stainless steel pipe Features

304 stainless steel has excellent corrosion resistance and good resistance to corrosion. 304 is most widely used stainless steel, heat-resistant steel and practical steel. It is mainly used for food production equipment, general chemical equipment, nuclear energy and so on.

Typical Chemical Properties of 304 stainless steel pipe

Carbon, Max %0.03
Manganese, Max %2.00
Phosphorus, Max %0.045
Sulphur, Max %0.03
Chromium, Max%17.5
Nickel, Min%8.0
Molybdenum, Max%N/A


Tensile Strength ksi81
Yield 2% Offset ksi37
Elongation in 2” (50.80mm)55

learn more:http://www.section-steel.com/News/304-stainless-steel-pipe-Manufacturing-Process.html
TEL:0086-21-61182423
Fax :0086-21-61182425
E-mail:service3@katalor.com
 

skype:lisa.liu6282

EN 10028 P355NL1 Pressure Vessel and Boiler Steel Plate Steel Grade


P355NL1 Chemical Composition

Grade
The Element Max (%)
C
Si
Mn
P
S
Al(min)
N
P355NL1
0.18
0.50
0.9-1.70
0.03
0.020

0.02
Cr
Cu
Mo
Nb
Ni
Ti
V
0.30
0.30
0.08
0.005
0.50
0.03
0.10
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
P355NL1Mechanical Property


Grade
Thickness
Yield
strength
Tensile
strength
Elongation
Impact Energy(KV J) min
P355NL1
mm
Min Mpa
Mpa
Min %
-20°
+20°
≤ 16
355
490-630
22
47
55
63
16> to ≤35
355
490-630
22
47
55
63
35> to ≤50
345
490-630
22
47
55
63
50> to ≤70
325
490-630
22
47
55
63
70> to ≤100
315
470-610
21
47
55
63
100> to ≤150
295
450-590
21
47
55
63

TEL:0086-21-61182423
Fax :0086-21-61182425
E-mail:service3@katalor.com  
skype:lisa.liu6282

2017年3月20日星期一

China Factory Price SA387GR11CL2 Press Vessel and Boiler Steel Plate


According to the different thickness and impact requirements, SA387 GR11CL2 steel plate's heat treatment choose normalized and tempered or normalized, accelerated cooling and tempered.

The Main Chemical Composition of SA387


Grade
Gr5 Cl2
Gr12 Cl2
Gr11 Cl2
Gr22 Cl2
Gr91
C
≤ 0.15
0.05-0.17
0.05-0.17
0.05-0.15
0.06-0.15
Mn
0.30-0.60
0.40-0.65
0.40-0.65
0.30-0.60
0.25-0.66
Si
≤ 0.50
0.15-0.40
0.50-0.80
≤ 0.50
0.18-0.56
P
≤ 0.035
≤ 0.035
≤ 0.035
≤ 0.035
≤ 0.020
S
≤ 0.035
≤ 0.035
≤ 0.035
≤ 0.035
≤ 0.010
Cr
4.00-6.00
0.80-1.15
1.00-1.50
2.00-2.50
8.00-9.50
Mo
0.45-0.65
0.45-0.60
0.45-0.60
0.90-1.10
0.85-1.05











SA387GR11CL2 Mechanical Property

Grade
Mechanical Property
Tensile Strength(MPa)
Yield Strength(MPa)
% Elongation in 2 in.(50mm) min
Impacting Test Temperature(°C)
SA387 Grade 11 Class2(SA387GR11CL2)
0.35-0.73
310
22
-20,40,-60











learn more:http://www.ice-steels.com/News/China-Factory-Price-SA387GR11CL2-Press-Vessel-and-Boiler-Steel-Plate.html
TEL:0086-21-61182423
Fax :0086-21-61182425
E-mail:service3@katalor.com
 

skype:lisa.liu6282